    How to repair iron casting defects?

    Cast Aluminum and Iron Parts Manufacturershare s that defects such as porosity, pinholes, slag inclusion, cracks and pits often occur in iron castings due to various factors.

    Common repair equipment for argon arc welding machine, resistance welding machine, cold welding machine.

    Casting defects with low quality and appearance requirements can be remedied by high heating and fast welding machines such as argon arc welding machines.

    However, in the field of defect repair of precision iron castings, due to the large influence of argon welding heat, the repair may cause secondary defects such as casting deformation, hardness reduction, sand hole, local annealing, cracking, pinhole, wear, scratch, undercut, or insufficient binding force and internal stress damage.

    Cold welding machine just to overcome the above shortcomings, its advantages are mainly reflected in the small heat affected area, casting without preheating, cold welding repair at room temperature, so no deformation, undercut and residual stress, no local annealing, does not change the metal structure of the casting state.

    Therefore, cold welding machine is suitable for precision casting surface defect repair.

    Cold welding welding repair in the range of 1.5 1.2 mm Φ Φ weld points repeatedly melting process of accumulation, in the process of large area of defect repair, repair efficiency is the only factor to restrict its wide application.

    For large defects, the composite application of traditional welding repair technology and casting defect repair machine is recommended.

    But sometimes we don't have a lot of defects, there would be no need to invest more costs, we can use some repairing adhesive repair good, convenient and simple, iron material, for example, we can use (strength element into) JS902 mending, can in the later use to burn, so can save cost for our factory, casting factory, let us get more money to improve the quality of the product itself, for the users to create more wealth.

    Welcome to purchase ourFurniture Iron Casting Parts!

    Located in Liaoning province in northeastern China, LianJiang Metals Company have specialized in aluminum and iron casting production since 1997 - We are an OEM partnership that manufactures Cast Aluminum and iron parts for clients all over the world and in different industries such as Street Lighting Base, patio furniture & Garden Decoration company.

    With over 20 years of casting work experience and expertise, we offer a full range of casting processes including: sand casting, gravity casting, die-casting, vacuum casting


    Company Contact:


    • Phone: +8641182637319

    • Address: 1812, International Building, No. 9 Renmin Road, Zhongshan District, Dalian, Liaoning, China, Dalian , Liaoning , China

    • Email: Email


    Published date: November 20, 2019

    • Business Description: Located in Liaoning province in northeastern China, LianJiang Metals Company have specialized in aluminum and iron casting production since 1997 - We are an OEM partnership that manufactures cast aluminum and iron parts for clients all over the world and in different industries such as street lighting, patio furniture & garden decoration company.

      With over 20 years of casting work experience and expertise, we offer a full range of casting processes including: sand casting,gravity casting,die-casting,vacuu m casting

    Related listings



    • Fireplace Art Shared
      Fireplace Art Shared
      Castings and casting assemblies - LianJiang Metals Company - China - November 20, 2019 - contact company for price

      Fireplace Art Shared By The Fireplace Casting Manufacturer Fireplace CastingManufacturer shares that in the west, fireplaces are also closely associated with various festivals. On Halloween, the most important ritual is to light a fire. As many small...

    • The Fireplace Symbolizes
      The Fireplace Symbolizes
      Castings and casting assemblies - LianJiang Metals Company - China - November 20, 2019 - contact company for price

      The Fireplace Symbolizes a Kind Of Status, Status And Style Fireplace Casting Manufacturershares that the appearance and use of fireplace is inseparable from the history of using fire. The use of fire is of great significance to the origin of human b...

    • Experience The Wonderful Fireplace Culture
      Experience The Wonderful Fireplace Culture
      Castings and casting assemblies - LianJiang Metals Company - China - November 20, 2019 - contact company for price

      The cold air swept in, and after a busy day back home, a warm room is the desire of all. In contemporary home outfit, fireplace serves supplied fromFireplace Casting Manufactureras the new bestow favor on household adornment in cold wintry day, it is...



    Safe Trade Tips

    • Ask for business references and check them
    • Use a payment method that offers better protection for all such as Letters of credit and verified professional escrow services. Avoid payments in advance such as money transfers
    • Verify their business via their local Chamber of Commerce
    • Search the internet using their website address, their business name, their phone and fax numbers, and their email addresses to see if you can find any feedback about them.
    • Get to know more about scams and fraud to avoid: Internet Crime Complaint Center - Consumer Financial Protection Bureau
    • This site is never involved in any transaction, and does not handle payments, shipping, guarantee transactions, provide escrow services, or offer "buyer protection" or "seller certification"